N2 wavesolder | 11 September, 1998

How can solve the small solder ball after w/s. (oxygen level is 40000~5000ppm, no-clean flux & Tamura N2 w/s machine).

reply »

Larry

#14346

Re: N2 wavesolder | 15 September, 1998

| How can solve the small solder ball after w/s. (oxygen level is 40000~5000ppm, no-clean flux & Tamura N2 w/s machine). Post your question in the SMT Forum for a better response. This area is not for tech questions.