Solder Joint Microstructure

blnorman

#24384

Solder Joint Microstructure | 1 May, 2003

What is the best way to determine solder joint intermetallic composition? Metallography? XDS of the joint? Any input is appreciated.

reply »

#24385

Solder Joint Microstructure | 1 May, 2003

Our first choice in determining the composition of metals would be to use Scanning Electron Microscopy (SEM) / Energy Dispersive Spectroscopy (EDS) analysis.

reply »


CAL

#24390

Solder Joint Microstructure | 1 May, 2003

Dave's point is right on the money. This would be a destructive test..needing microsectioning.

Cal Communications Test Design, Inc

reply »


CAL

#24391

Solder Joint Microstructure | 1 May, 2003

Dave's point is right on the money. This would be a destructive test..needing microsectioning.

Cal Communications Test Design, Inc

reply »

#24392

Solder Joint Microstructure | 2 May, 2003

Bill

Why do you want to do this analysis? There are limited IMC that can form.

reply »