Hello all,

I am looking for a high temp lead free solder wire to use when attaching thermocouples for oven profiling. I figure something that reflows at 270-300c would do the trick. Can anyone give me a Brand, model# for such a solder?

THANKS.

reply »

#40111

Lead Free High Temp Solder Wire | 2 March, 2006

HMP solders Pb >85% are exempt from the RoHS directive. Doesn't make a lot of sense but that wasn't your question.

reply »


RDR

#40125

Lead Free High Temp Solder Wire | 2 March, 2006

Your best bet would be to browse through you current solder suppliers catalog and pick your alloy. Most of them have a list of alloys and their melting points as well as what form they can be supplied in.

reply »

Slaine

#40336

Lead Free High Temp Solder Wire | 10 March, 2006

Multicore make a HMP alloy liquidus at 298 degrees, Pb93Sn5Ag2.Ive used it to attatch thermocouples but they're difficult to solder as they dont wet.