Electronics Forum | Fri Apr 30 08:44:46 EDT 1999 | Dave F
| | | | | | Has anyone heard of this company? We have one at our facility and I can't find them listed anywhere. I looked through this years NEPCON directory with no listing there either. We have some parts that need replacing so any help would be
Electronics Forum | Tue Apr 27 16:44:05 EDT 1999 | Chrys Shea
| | Has anybody had experience wavesoldering 1 watt 2512 resistor packages?? I know it can be done, but are there reliability issues? | | | | We are in the middle of a new product and the question was posed to me "Can we use 2512 1 watt resistors o
Electronics Forum | Thu Apr 29 16:56:16 EDT 1999 | Kevin Hussey
| | We are an assembly house engaged in large volume manufacturing of Computer motherboards and others. We are in the process of selection of a new wave soldering machine. Can somebody help me inform what are the different parameters which must be e
Electronics Forum | Wed Apr 21 00:35:31 EDT 1999 | Scott Cook
| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185
Electronics Forum | Tue Mar 16 14:23:44 EST 1999 | Steve Skinner
| Does anyone have any recommendations on spray fluxers? Are there major differences between the high priced ultrasonic machines to the low priced flux/air spraying machines? We are going to be spraying an OA flux with 11% solids content. Are there a
Electronics Forum | Mon Mar 29 16:56:58 EST 1999 | Chrys Shea
| | Does anyone have any recommendations on spray fluxers? Are there major differences between the high priced ultrasonic machines to the low priced flux/air spraying machines? We are going to be spraying an OA flux with 11% solids content. Are there
Electronics Forum | Wed Jan 20 21:25:32 EST 1999 | Tony A
| I get white residue on my PCBs after vapor degreasing. No comments on the vapor degreaser. Yes, I still use one of these. I use a vapor degreaser and a 1,1,1 replacement solvent due to the quick clean and quick dry times. Anyway, I only get whi
Electronics Forum | Tue Jan 12 08:47:39 EST 1999 | Dick Casagrande
| | | I need leads on equipment vendors for selective soldering systems. I have information about ERSA and Seho already. I want to contact Air Vac in particular, but I can't find thier phone number. Thanks for the help | | | | | Jim, | | | | Be
Electronics Forum | Tue Jan 12 09:29:37 EST 1999 | Dave F
| | | We are currently fighting a dross battle on our non-inerted waves. We are currently using a bar solder that barely meets QQS-571 for Alloy/Impurity. | | | | | | Is anybody using HI FLO in a non inerted wave? Do you see a measureable decrease
Electronics Forum | Fri Nov 27 13:04:47 EST 1998 | Phillip Hunter
| Hi | I have been conducting my first reflow profiles. Most of the texts that I have read suggest soldering the thermocouples to a populated pcb. I am finding this very difficult. I have been using a high melting point (Sn5 / Pb95) solder and the