Condensation Soldering

Electronics Forum | Fri Oct 19 01:33:30 EDT 2001 | ianchan

Hi, Encountered this deference to the vapour phase process that was supposedly "phased" out years ago? *pardon the pun* Any comments from folks who have used this proces before? how about folks who are currently using this process? even better, a

AXI and AOI

Electronics Forum | Tue Jul 09 15:20:19 EDT 2002 | pjc

When you look at the capabilities of Combo machines they tend to sacrifice performance when compared to separate X-ray and AOI machines, meaning they don't do either the X-ray or AOI operations as well as a machine that was designed to do only one. A

Capability Process CPk

Electronics Forum | Mon Mar 10 15:52:26 EST 2003 | eagle-eyed-one

Hello Neil, I absolutely agree with the conclusion of limits as you have stated. There are 2 sets of limits in which machines can be measured against for compliant performance. First and most critical being the quality performance specification limit

Automatic Paste Inspection worth it?

Electronics Forum | Fri Mar 14 17:41:32 EDT 2008 | jerrysaise

Hello Before I say anything. Here is one caveat, I work for a 3D paste inspection vendor, I will not mention which. So you can take whatever I say with a grain of salt. Paste inspection will make a difference if you want to put the effort into it ma

Selective moving pot vs fixed pot

Electronics Forum | Thu Jul 10 13:34:43 EDT 2008 | rwyman

We have a Vitronics mySelective machine (model 6749, or "the Fat Bastard" as we affectionately call it). It's configurable with various combinations of "select wave" and "multi wave" pots. Ours has one of each. The "select wave" is for the most pa

Flux residues

Electronics Forum | Thu Nov 15 15:27:50 EST 2012 | davef

Finally, help for those searching for compatibility A new standard and guideline will make it much simpler for users to determine whether they’ve got the right chemistry to ensure compatibility. April 23, 2012 By Terry Costlow, IPC online edit

Re: Poor HASL Finish known to cause solder shorts?

Electronics Forum | Fri Sep 24 10:57:18 EDT 1999 | Earl Moon

| Hi Folks: | | We've been having bridging problems on our fine-pitch QFP's, despite thorough inspection of paste height, volume, and placement accuracies....profiles look good also. | | The bridging is happening after coming out of reflow...one la

Re: Moisture sensitive device processing

Electronics Forum | Sun Apr 25 04:12:34 EDT 1999 | Earl Moon

| At Sanders (Military manufacturer), we have only started using plastic parts within the past few years. After being tasked with reviewing the new J-Std-033, it became obvious to me our process for controlling device exposure is weak. We build very

Re: DPM-Rate for SMT pprocess

Electronics Forum | Thu Oct 08 22:06:44 EDT 1998 | Eric R

| | | Does sombbody know what DPM rate a good and reliable SMT assembly line (incl. solder paste print, assembly and feflow soldering) has? | | | DPM is Defects per million, usually measured on components. We run a process consisting of small to medi

Design of Experiments

Electronics Forum | Fri Jun 26 08:58:43 EDT 1998 | Justin Medernach

| WHAT IS THE BEST ANGLE FOR THE SQUEEGEE BLADE TO BE ANGLED AT? WE ARE USING 45 DEGREE ON OUR POLYURETHANE BLADES, AND I BELIVE WE HAVE THE OPTION OF EITHER 45 OR 60 DEGREES ON OUR METAL BLADES. WHICH OF THE TWO IS BETTER, OR SHOULD WE BE USING AN