Low Melting Temperature Sn-Bi Solder: Effect of Alloying and Nanoparticle Addition on the Microstructural, Thermal, Interfacial Bonding, and Mechanical Characteristics
Published: |
May 13, 2021 |
Author: |
Hyejun Kang, Sri Harini Rajendran and Jae Pil Jung |
Abstract: |
Sn-based lead-free solders such as Sn-Ag-Cu, Sn-Cu, and Sn-Bi have been used extensively for a long time in the electronic packaging field. Recently, low-temperature Sn-Bi solder alloys attract much attention from industries for flexible printed circuit board (FPCB) applications. Low melting temperatures of Sn-Bi solders avoid warpage wherein printed circuit board and electronic parts deform or deviate from the initial state due to their thermal mismatch during soldering. However, the addition of alloying elements and nanoparticles Sn-Bi solders improves the melting temperature, wettability, microstructure, and mechanical properties. Improving the brittleness of the eutecticSn-58wt%Bi solder alloy by grain refinement of the Bi-phase becomes a hot topic. In this paper, literature studies about melting temperature, microstructure, inter-metallic thickness, and mechanical properties of Sn-Bi solder alloys upon alloying and nanoparticle addition are reviewed... |
You must be a registered user to talk back to us. |
Company Information:
More SMT / PCB assembly technical articles »
- Aug 20, 2024 - Thermal Interface Materials Drive Electronic Innovation | GPD Global
- Aug 20, 2024 - Underfill Materials Dispensing in Electronics Manufacturing Applications | GPD Global
- Jul 15, 2024 - Transforming LED Manufacturing: I.C.T Engineers Set Up Complete Production Line in Tajikistan | I.C.T ( Dongguan ICT Technology Co., Ltd. )
- Jun 20, 2024 - Case study: Precise Coating on Electronic Hearing Devices | ASYMTEK Products | Nordson Electronics Solutions
- Mar 19, 2024 - What is Underfill | GPD Global
- Browse Technical Library »
Low Melting Temperature Sn-Bi Solder: Effect of Alloying and Nanoparticle Addition on the Microstructural, Thermal, Interfacial Bonding, and Mechanical Characteristics article has been viewed 534 times